Dow Corning SE 1885 KIT

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SE 1885 KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, clear, 1:1, addition cure, low temperature cure, low temperature capable, low viscosity.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Viscosity 400 cP
400 cP
dynamic
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 90
90
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -80.0 °C
-112 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.7

@Frequency 1.00e+6 Hz
2.7

@Frequency 1.00e+6 Hz
Dielectric Strength 17.0 kV/mm
432 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 70.0 °C
0.500 hour

@Temperature 158 °F
Shelf Life 17.0 Month
17.0 Month
Descriptive Properties Value Comments
Appearance clear
Flowable yes
Gel Hardness (Grams/Penetration) 50
Hydrophobic yes
Self Leveling yes
Water Resistant yes
Working Time (min) 60