Material Notes:
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextrusion equipment designed+F47 to process polyethylene resins. Physical properties of BYNEL Series 4100 resins are typical of linear low-density polyethylene resins with similar density and melt index values. Use of these adhesive resins in coextruded PE/barrier structures offers improved thermal resistance over that of ethylene vinyl acetate-based adhesive resins. BYNEL 4100 series resins adhere to a variety of materials. They are most often used to adhere to EVOH, polyamide, PE and ethylene copolymers. Series 4100 resins can be used in coextrusion processes including: blown film cast film/sheet blow molding melt and solid phase thermoforming sheet and tubing LLDPE resins are known for their temperature resistance, clarity and toughness. These physical properties make the 4100 series resins work well in applications such as: boil-in-bag structures blow molded containers in which drop strength is important bag-in-box films film where LLDPE is the heat seal layer
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792, ISO 1183
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 103 °C
217 °F
Freezing Point; ASTM D3418
120 °C
248 °F
ASTM D3418, ISO 3146
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 260 °C
<= 500 °F
Feed Temperature 160 °C
320 °F
CoExtrusion with EVOH Processing
160 °C
320 °F
CoExtrusion with Nylon Processing
Zone 2 185 °C
365 °F
CoExtrusion with EVOH Processing
185 °C
365 °F
CoExtrusion with Nylon Processing
Zone 3 235 °C
455 °F
CoExtrusion with EVOH Processing
235 °C
455 °F
CoExtrusion with Nylon Processing
Zone 4 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Zone 5 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Adapter Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Die Temperature 235 °C
455 °F
CoExtrusion with EVOH Processing
260 °C
500 °F
CoExtrusion with Nylon Processing
Melt Temperature 210 - 235 °C
410 - 455 °F
CoExtrusion with EVOH Processing
<= 260 °C
<= 500 °F
CoExtrusion with Nylon Processing
Users viewing this material also viewed the following: