DuPont Performance Polymers Crastin® CE2061 BK560 PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® CE2061 BK560 PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crastin® CE2061 is a 20% glass reinforced polybutylene terephthalate with high melt viscosity designed for blow molding.Information provided by DuPont
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Filler Content 20 %
20 %
Water Absorption 0.40 %

@Temperature 23.0 °C
0.40 %

@Temperature 73.4 °F
Saturation, immersed; ISO 62, Similar to
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa

@Temperature 23.0 °C
13800 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 2.9 %

@Temperature 23.0 °C
2.9 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 6.20 GPa

@Temperature 23.0 °C
899 ksi

@Temperature 73.4 °F
ISO 527
Processing Properties Metric English Comments
Melt Temperature 222 °C
432 °F
Optimum; Blow Molding
240 - 260 °C
464 - 500 °F
Blow Molding
Drying Temperature 120 °C
248 °F
Blow Molding
Dry Time 4.00 hour
4.00 hour
Dehumidified Dryer; Blow Molding
Moisture Content 0.40 %
0.40 %
Blow Molding
Descriptive Properties Value Comments
Appearance Black Color
Drying Recommended Yes
Blow Molding
Features Viscosity, High
Filler Glass Reinforced
Generic PBT
Material Status Preliminary Data
Part Marking Code >PBT-GF20<
ISO 11469
Processing Method Blow Moldable
Product Category Blow Moldable Resins
Glass Reinforced Resins
Region Available - Americas Yes
Region Available - Asia/Pacific Yes
Region Available - Europe Yes
Resin Identification PBT-GF20
ISO 1043
RoHS Compliance Contact Manufacturer
Uses Blow Molding Applications