Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Hytrel® HTR8539 BK316 TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® HTR8539 BK316 TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hytrel® HTR8539 is a 72 Shore D, plasticiser free, high performance resin for extrusion. It has high viscosity.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Melt Flow 7.5 g/10 min

@Load 10.0 kg,
Temperature 250 °C
7.5 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 70

@Time 15.0 sec
70

@Time 0.00417 hour
ISO 868
Tensile Strength at Break 40.0 MPa

@Temperature 23.0 °C
5800 psi

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Stress 30.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
4350 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
Elongation at Break 200 %

@Temperature 23.0 °C
200 %

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Modulus 0.900 GPa

@Temperature 23.0 °C
131 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 217 °C
423 °F
10°C/min; ISO 11357-1/-3
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974
Processing Properties Metric English Comments
Melt Temperature 250 °C
482 °F
Optimum; Extrusion
Drying Temperature 100 - 130 °C
212 - 266 °F
Extrusion
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Extrusion
Moisture Content <= 0.060 %
<= 0.060 %
Extrusion
Descriptive Properties Value Comments
Generic TPC-ET
Part Marking Code >TPC-ET+PBT<
ISO 11469
Product Category Extrusion Resins
Resin Identification TPC-ET+PBT
ISO 1043