Physical Properties Metric English Comments
Density 1.70 - 2.00 g/cc
0.0614 - 0.0723 lb/in³
Average value: 1.86 g/cc Grade Count:14
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..
Density 1.25 - 2.00 g/cc
0.0452 - 0.0723 lb/in³
Average value: 1.74 g/cc Grade Count:7
Overview of materials for Phenolic/Glass Fiber SMC
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appro..
Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1..
Density 1.85 - 2.00 g/cc

@Temperature 25.0 °C
0.0668 - 0.0723 lb/in³

@Temperature 77.0 °F
Hong Kun Group APP (Phase II) Flame Retardant
Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
molded; ASTM D792
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite
PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w..
Density 1.60 - 2.00 g/cc
0.0578 - 0.0723 lb/in³
Tap
Solvay CEROXâ„¢ 1650 Surfactant
Description: Ceroxâ„¢1650 offers an optimized polishing performance for optical and ophthalmic lenses as well as for other demanding applications like photomask and glass hard disks. Benefits: Hi..
Density 1.60 - 2.00 g/cc
0.0578 - 0.0723 lb/in³
Tap
Solvay SUPER CEROXâ„¢ 1663 Surfactant
Description: Super Ceroxâ„¢1663 is particularly suited for the polishing of ophthalmic lenses (mass production and prescription) and optical lenses. Benefits: High polishing efficiency, Very high..
Density 1.96 - 2.00 g/cc
0.0708 - 0.0723 lb/in³
ISO R 1183
Fainplast Compounds CRA 84 Flexible PVC, Flame Retardant Electrical Bedding
Flame retardant bedding
Density 1.00 - 2.00 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.0361 - 0.0723 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
BASF Palusol® SW 60-1 FSC 100% Silicate Panel
Information provided by BASF
Density 1.80 - 2.00 g/cc
0.0650 - 0.0723 lb/in³
ISO 1138
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound
Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm..
Density 1.80 - 2.00 g/cc
0.0650 - 0.0723 lb/in³
ISO 1138
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound
UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot..
Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
ISO 1138
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound
Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion..
Density 1.80 - 2.00 g/cc
0.0650 - 0.0723 lb/in³
ISO 1138
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound
Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p..
Density 0.917 - 2.00 g/cc
0.0331 - 0.0723 lb/in³
Average value: 0.988 g/cc Grade Count:76
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer
A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties...
Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer
A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen..
Density 1.90 - 2.00 g/cc
0.0686 - 0.0723 lb/in³
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application..