Download PDF DuPont Performance Polymers Rynite® 530HTE NC010 Polyethylene Terephthalate (PET)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced Polyethylene Terephthalate with Excellent High Temperature Dielectric PropertiesRynite 530HTE NC010 is a 30% glass reinforced modified polyethylene terephthalate resin with excellent high temperature dielectric properties.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 280 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 536 °F
cm³/10min; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
ASTM D785
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 170 MPa
24700 psi
ISO 527-1/-2
Elongation at Break 2.3 %
2.3 %
ISO 527-1/-2
2.3 %
2.3 %
ASTM D638
Tensile Modulus 10.7 GPa
1550 ksi
ASTM D638
11.0 GPa
1600 ksi
ISO 527-1/-2
Izod Impact, Unnotched (ISO) 695 kJ/m²
331 ft-lb/in²
ASTM D4812
Izod Impact Resistance 9.00 J/cm²
42.8 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
Dielectric Constant 4.1

@Frequency 1.00e+6 Hz
4.1

@Frequency 1.00e+6 Hz
ASTM D150
4.2

@Frequency 1000 Hz
4.2

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 34.0 kV/mm
864 kV/in
IEC 60243-1
Dissipation Factor 0.0040

@Frequency 1000 Hz
0.0040

@Frequency 1000 Hz
ASTM D150
0.014

@Frequency 1.00e+6 Hz
0.014

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >PET-GF30<
ISO 11469
Processing Injection Moulding
Regional Availability Europe
Near East/Africa
North America
South and Central America
Resin Identification PET-GF30
Special Characteristics Heat stabilised or stable to heat
UL recognition UL
Users viewing this material also viewed the following: