E-Polymers TEKANATE® G7038 High Easy Molding Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKANATE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKANATE® G7038 High Easy Molding Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified Poly Carbonate: TEKANATE is a modified PC by improving polycarbonate resins with features of halogen-free flammability, transparency, impact resistance and reinforced fiberglass. It shows high dimensional stability and rigidity.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Melt Flow 38 g/10 min

@Load 1.20 kg,
Temperature 300 °C
38 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 61.41 MPa
8907 psi
ASTM D638
Elongation at Break 135 %
135 %
ASTM D638
Flexural Strength 91.04 MPa
13200 psi
ASTM D790
Flexural Modulus 2.091 GPa
303.2 ksi
ASTM D790
Izod Impact, Notched 8.83 J/cm
16.5 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 130 °C
>= 266 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Melt Temperature 270 - 300 °C
518 - 572 °F
Mold Temperature 80.0 °C
176 °F