Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ELASTO UK Dryflex® 602900S SEBS Based Material, Filled Qualities, 90A Hardness, Black

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 602900S SEBS Based Material, Filled Qualities, 90A Hardness, Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material reduced that stickiness and sink marks on thick details but has limited scratch resistance. Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.020 cm/cm
0.0080 - 0.020 in/in
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90

@Thickness 4.00 mm
90

@Thickness 0.157 in
ASTM D2240
Tensile Strength at Break 13.0 MPa
1890 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
100% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
300% Modulus 0.00600 GPa
0.870 ksi
ASTM D638
Tear Strength 50.0 kN/m
285 pli
ASTM D624
Compression Set 34 %
34 %
at 23°C, 72 hrs; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Processing Properties Metric English Comments
Processing Temperature 180 - 210 °C
356 - 410 °F
Descriptive Properties Value Comments
Bonding to PP Excellent
Chemical Resistance Good
Excluding organic solvents, aromatic and vegetable oils
Color Black
Weather Resistance Excellent
Air ageing
Users viewing this material also viewed the following: