EMS-Grivory Grivory® L 25A NZ PA12-I

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® L 25A NZ PA12-I.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid L 25A NZ are: Very good hydrolysis resistanceGood heat stabilityGood low temperature impact strengthGood chemical resistanceHigh surface finishGood dimensional stabilityHigh processing speedsLow density, low weight Application examples: Grilamid L 25A NZ is suitable for the extrusion of profiles and tubes for applications in automotive and industrial markets.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Water Absorption 1.3 %
1.3 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
conditioned, 15s; ISO 868
Tensile Strength at Break 40.0 MPa
5800 psi
conditioned; ISO 527-1/-2
45.0 MPa
6530 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 30.0 MPa
4350 psi
dry; ISO 527-1/-2
35.0 MPa
5080 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 12 %
12 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.750 GPa
109 ksi
conditioned; ISO 527-1/-2
1.00 GPa
145 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
dry; ISO 179/1eA
10.0 J/cm²
47.6 ft-lb/in²
conditioned; ISO 179/1eA
7.50 J/cm²

@Temperature 30.0 °C
35.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
8.00 J/cm²

@Temperature 30.0 °C
38.1 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 100 °C
194 - 212 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Descriptive Properties Value Comments
Automotive Air intake sytems
Compressed air systems
Cooling and climate control
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Sports & Leisure
Processing Injection Molding
Other Extrusion
Product Attributes High viscosity
Hydrolysis resistant
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)