EMS-Grivory Grivory® TSZ 1 PA666

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TSZ 1 PA666.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon TSZ 1 is a heat stabilized, normal viscosity, impact modified PA66 + PA6 injection molding grade. Grilon TSZ 1 has the following important properties: Excellent flow behaviorHigh elongation at breakIntegral hinge suitableGood surface finish Grilon TSZ 1 is used typically for automotive and electro applications such as clips, fixing parts, cable conduits, cable binders, and head rest bushings.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Water Absorption 8.5 %
8.5 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.012 cm/cm
0.012 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 45.0 MPa
6530 psi
conditioned; ISO 2039-1
125 MPa
18100 psi
dry; ISO 2039-1
Tensile Strength at Break 40.0 MPa
5800 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 35.0 MPa
5080 psi
dry; ISO 527-1/-2
65.0 MPa
9430 psi
dry; ISO 527-1/-2
Elongation at Break 25 %
25 %
dry; ISO 527-1/-2
25 %
25 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
dry; ISO 527-1/-2
20 %
20 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.750 GPa
109 ksi
conditioned; ISO 527-1/-2
2.40 GPa
348 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
dry; ISO 179/1eA
4.50 J/cm²
21.4 ft-lb/in²
conditioned; ISO 179/1eA
0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°C
83.3 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
conditioned; IEC 60243-1
31.0 kV/mm
787 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Electricals & Electronics Connectors
Form Granules
Industry & Consumer goods Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Special Characteristics High impact or impact modified