Material Notes:
VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET food packaging made from VersaTray plastic is dual ovenable, which means it can be used in either a microwave or a conventional oven. So it gives you the most heating and cooking flexibility. You can heat, bake, warm or brown your meal in either appliance. And, CPET trays are also freezable. Applications/UsesCrystallized PET (CPET) traysDual ovenable containersFood packagingFood-contact applicationsKey AttributesDual ovenableHigh temperature food packaging
Physical Properties Metric English Comments
Bulk Density 0.800 g/cc
0.0289 lb/in³
Poured; ASTM D1895
0.855 g/cc
0.0309 lb/in³
Vibrated; ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.92 - 0.98
0.92 - 0.98
Intrinsic; VGAS-A-AN-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 59.0 J/g
25.4 BTU/lb
ASTM E793
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
ASTM E1269
1.30 J/g-°C

@Temperature 80.0 °C
0.311 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.40 J/g-°C

@Temperature 100 °C
0.335 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.80 J/g-°C

@Temperature 200 °C
0.430 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.00 J/g-°C

@Temperature 280 °C
0.478 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 250 °C
482 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <3ppm
VKCA-A-AS-G-GC-0001
Color, CIE a* -2.7 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE b* 0.9 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE L* 75.5 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.05
Pellet Shape Cubical
Users viewing this material also viewed the following: