Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 4703ZD84 Tungsten Filled Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 4703ZD84 Tungsten Filled Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 5.60 g/cc
5.60 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 590 %
590 %
ASTM D638
Tensile Modulus 0.621 GPa
90.0 ksi
ASTM D638
Flexural Strength 55.2 MPa
8000 psi
ASTM D790
Flexural Modulus 0.0965 GPa
14.0 ksi
ASTM D790
Izod Impact, Notched 3.95 J/cm
7.40 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 204 - 221 °C
400 - 430 °F
Mold Temperature 10.0 - 26.7 °C
50.0 - 80.0 °F
Drying Temperature 93.3 °C
200 °F
then reduce to 160°F
Dry Time 2 hour
2 hour