Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 102 microns
4.00 mil
Layer 1; Arlon SQA-TMS-003
178 microns
7.00 mil
Layer 2; Arlon SQA-TMS-003
457 microns
18.0 mil
Substrate
737 microns
29.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
Silicone Property; ASTM D2240
Tensile Strength 7.93 MPa
1150 psi
Silicone Property; ASTM D412
Elongation at Break 350 %
350 %
Silicone Property; ASTM D412
Tear Strength 16.7 kN/m
95.0 pli
Silicone Property; ASTM D6242
Peel Strength 2.77 kN/m
15.8 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 HB
HB
at 220°C per card E54153
Electrical Properties Metric English Comments
Dielectric Strength 14.6 kV/mm
370 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 31.5
Arlon SQA-TMS-025