Entec Hylox® 9020 PBT, 20% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer Entec Engineered Resins
Trade Name Hylox®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hylox® 9020 PBT, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 124 MPa
18000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
73°F; ASTM D256
Processing Properties Metric English Comments
Rear Barrel Temperature 232 - 243 °C
450 - 470 °F
Middle Barrel Temperature 238 - 249 °C
460 - 480 °F
Front Barrel Temperature 243 - 254 °C
470 - 490 °F
Nozzle Temperature 243 - 254 °C
470 - 490 °F
Melt Temperature 249 - 260 °C
480 - 500 °F
Mold Temperature 82.2 - 121 °C
180 - 250 °F
Drying Temperature 121 °C
250 °F
Dry Time <= 12 hour
<= 12 hour
Moisture Content <= 0.020 %
<= 0.020 %
Injection Pressure 6.89 - 11.7 MPa
1000 - 1700 psi
Back Pressure 0.138 - 0.414 MPa
20.0 - 60.0 psi
Shot Size 40 - 80 %
40 - 80 %
Screw Speed 40 - 80 rpm
40 - 80 rpm
Descriptive Properties Value Comments
Injection Rate Moderate-Fast