Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Eurostar Engineering Plastics
Trade Name Star L
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Star L PA66 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 4.00 mm
0.0030 - 0.0050 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 165 MPa
23900 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Flexural Strength 219 MPa
31800 psi
ISO 178
Flexural Modulus 8.00 GPa
1160 ksi
ISO 178
Izod Impact, Notched (ISO) 8.20 kJ/m²
3.90 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 38.0 kJ/m²
18.1 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Melting Point 264 °C
507 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 236 °C
457 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 265 - 275 °C
509 - 527 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 270 - 280 °C
518 - 536 °F
Melt Temperature 270 - 280 °C
518 - 536 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.20 %
0.20 %