ExxonMobil NTX™ NTX 141 Super Strength Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Exxon Chemical
Trade Name NTX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil NTX™ NTX 141 Super Strength Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impact and tear strength. NTX resins are formulated with various additive packages for use in all high performance film applications.Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
Antiblock Level 6500 ppm
6500 ppm
Slip Level 1400 ppm
1400 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.3 MPa
1500 psi
ASTM D882
Film Tensile Strength at Yield, TD 10.3 MPa
1500 psi
ASTM D882
Film Elongation at Break, MD 565 %
565 %
ASTM D882
Film Elongation at Break, TD 775 %
775 %
ASTM D882
Elmendorf Tear Strength, MD 16.9 g/micron
430 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 29.5 g/micron
750 g/mil
ASTM D1922
Dart Drop 18.9 g/micron
480 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 55.2 MPa
8000 psi
ASTM D882
Film Tensile Strength at Break, TD 40.0 MPa
5800 psi
ASTM D882
1% Secant Modulus, MD 193 MPa
28000 psi
ASTM D882
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Descriptive Properties Value Comments
Features Thermal Stabilizer