ExxonMobil PP7033L1 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP7033L1 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: An impact copolymer resin characterized with low flow. It is suitable for extrusion applications like sheet and thermoforming. It is also suitable for molding applications like boxes, buckets, containers and crates and other consumer and industrial applications.Availability: Africa & Middle East and Europe Features: Low Flow Uses: Consumer ApplicationsContainers Industrial ApplicationsTool/Tote BoxProcessing Method: Injection Molding, Sheet Extrusion and ThermoformingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2/50
Elongation at Yield 9.0 %
9.0 %
ISO 527-2/50
Tensile Modulus 1.10 GPa
160 ksi
ISO527-2/1
Flexural Modulus 1.00 GPa
145 ksi
Secant; ISO 178
Izod Impact, Notched (ISO) 7.56 kJ/m²
3.60 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.399 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.504 J/cm²

@Temperature 0.000 °C
2.40 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
1.05 J/cm²

@Temperature 22.8 °C
5.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 322 °C
612 °F
ISO 3146
Crystallization Temperature 235 °C
455 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 76.1 °C
169 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 47.2 °C
117 °F
ISO 75-2/A
Vicat Softening Point 146 °C
295 °F
ISO 306/A50