Fainplast Compounds PG 58/K1-UV Flexible PVC, Extrusion Modified with Rubber

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PG 58/K1-UV Flexible PVC, Extrusion Modified with Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Gaskets mat finish UV-Resistant
Physical Properties Metric English Comments
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 56 - 60
56 - 60
ISO R 868
Tensile Strength at Break 10.0 MPa
1450 psi
ISO R 527
Elongation at Break 300 %
300 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -40.0 °C
-40.0 °F
Cold Flex; ISO 458/2