Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)

Category Ceramic , Glass , Oxide , Silicon Oxide
Manufacturer Ferro Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to achieve very low alkali and iron levels and can be applied by a variety of techniques including photo-spin, spin coat, doctor blading, sedimentation, screen printing, and electrophoresis.Information provided by Ferro Corporation
Physical Properties Metric English Comments
Density 3.81 g/cc
0.138 lb/in³
Particle Size 1.5 µm
1.5 µm
50% of particles, (SRRG Powder)
3.0 µm
3.0 µm
50% of particles, (RWG Powder)
7.0 µm
7.0 µm
50% of particles, (REG Powder)
9.0 µm
9.0 µm
50% of particles, (TF Powder)
<= 10 µm
<= 10 µm
SRRG Powder
<= 25 µm
<= 25 µm
RWG Powder
<= 75 µm
<= 75 µm
REG Powder
<= 75 µm
<= 75 µm
TF Powder
Thermal Properties Metric English Comments
CTE, linear 4.35 µm/m-°C

@Temperature 25.0 - 260 °C
2.42 µin/in-°F

@Temperature 77.0 - 500 °F
Softening Point 825 °C
1520 °F
Transformation Temperature 620 °C
1150 °F
Chemical Properties Metric English Comments
Ionic Impurities - Na (Sodium) <= 30 ppm
<= 30 ppm
TF, REG Powders
<= 50 ppm
<= 50 ppm
RWG, SRRG Powders
Ionic Impurities - K (Potassium) <= 10 ppm
<= 10 ppm
TF, REG Powders
<= 30 ppm
<= 30 ppm
RWG, SRRG Powders
Processing Properties Metric English Comments
Processing Temperature <= 150 °C
<= 302 °F
Maximum Junction Temperature
860 °C
1580 °F
Typical Firing Temperature; Typical Firing Time: 10-20 min. at Peak
Descriptive Properties Value Comments
Ionic Impurities - Li (Lithium) ppm, Max 10
RWG, SRRG Powders
10
TF, REG Powders
Users viewing this material also viewed the following: