Material Notes:
TPO copolymer, UL certified, and FDA compliant.Features: Structural stiffness, ultra high impact strength, and high uniform flow rate.Applications: Injection molding: automotive items and exterior equipment components.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 40
40
ASTM D785
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Yield 30 %
30 %
ASTM D638
Flexural Modulus 0.850 GPa
123 ksi
Tangent; ASTM D790
Gardner Impact >= 36.0 J

@Temperature -30.0 °C
>= 26.6 ft-lb

@Temperature -22.0 °F
ASTM D3029
Impact Test 23.0 J

@Temperature -30.0 °C
17.0 ft-lb

@Temperature -22.0 °F
Multi-axial Impact; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM D648