Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Multibase Multi-Pro® 2010 M Polypropylene Mica Filled, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Multibase Multi-Pro® 4006 TH Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
ExxonMobil HD 9856BA Blow Molding Resin
(discontinued **) HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracki.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Global CPP-110 10% CaC03 Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 30.3 MPa @Temperature 23.0 °C |
4400 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos L06Z-00 Polypropylene Impact Copolymer This is a medium MFR impact copolymer polypropylene made for injection molded caps and closures applications. It offers a good balance of stiffness to impact resistance as compared to other impact .. |
|||
Tensile Strength, Yield | 30.34 MPa | 4400 psi | ASTM D638 |
Lucent Polymers CPP-110 Polypropylene Homopolymer, 10% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Kostat ICP-STAT ICD-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Techmer ES HiFill® HDPE TM30 30% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Spartech EP5220 Calcium Carbonate Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Calcium Carbonate filled grades offer an excellent balance of stiffness and impact resistance. Typical applications inc.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Spartech PE4312 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Spartech Royalstatâ„¢ R64 HDPE Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 3335N Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3335N is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for thin walled, injec.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Westlake Plastics Propylux® SD-A Polypropylene (anti-static) Non-carbon-filled, permanently static-dissipative material, with good chemical resistance and mechanical properties. This material is light weight, weldable, easily machined and fabricated, availab.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | 2" (50mm) per min.; ASTM D638 Type IV |
Formosa Plastics Formolene® HB6007 Blow Molding HDPE HomopolymerApplications: Milk, distilled water, soft drink concentrate, fruit juice, etc.Formolene HB6007 is a high quality product for those critical food packaging requirements. It also has excell.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 3312B Random Copolymer Polypropylene Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3312B is a medium melt flow random copolymer with fast cycle time and easy mold release. It is designed for injection moldin.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | 2" (50mm) per min, Type IV; ASTM D638 |
Formosa Plastics Formolene® HP6000 Pipe HDPE High Density Polyethylene Homopolymer for Pipe Extrusion Formolene® HP6000 is a high quality product for homopolymer pipe extrusion applications. It has excellent stiffness and good stiffness prope.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
ExxonMobil HDPE HD 9856B High Density Polyethylene Resin Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Clariant ABSSP0004 ABS, Chemical Resistant Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
ExxonMobil HD 9856B Blow Molding Resin Product Description: HD 9856B is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856B exhibit a unique combination of stiffness and environme.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | ASTM D638 |
Asahi Kasei Thermylene® P-20-0739 20% Talc Filled, High Impact, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 30.3 MPa | 4400 psi | 2" per min, Type IV; ASTM D638 |
Amco PRIMATOP HDPE 006964 Blow Molding Polyethylene HDPE 004955HP features excellent stiffness to ESCR ratio and good impact resistance. Applications include oil bottles, household and industrial chemical containers, and personal care products.Former.. |