Formosa Plastics Formolene® HL5505 Blow Molding HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® HL5505 Blow Molding HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extra High Molecular Weight CopolymerApplications: 55 gallon drums (even those with demanding built-in handling rings), industrial tanksFormolene HL5505 is intended for large part blow molding applications. Besides having excellent chemical resistance properties HL5505 HDPE has outstanding environmental stress crack resistance properties, and exceptional impact and creep resistance.Formolene HL5505 meets all requirements of ASTM D1248 - Type II, Category 5.Formolene HL5505 meets all requirements of ASTM - Type III, Category 5 and ASTM 4967-89-PE235.Produced using licensor formulation for HXM TR-570. Licensor does not warrant or imply that this product meets their specifications for HXM TR-570.Nominal properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928. Physical properties are typical of product but do not reflect normal testing variance and therefore should not be used for specification purposes.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693
>= 1000 hour
>= 1000 hour
Condition B (10% Igepal), F<sub>50</sub>; ASTM D1693
High Load Melt Index 5.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
5.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
2" (50mm) per min.; ASTM D638 Type IV
Elongation at Break >= 600 %
>= 600 %
2" (50mm) per min.; ASTM D638 Type IV
Flexural Modulus 1.34 GPa
195 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -83.9 °C
<= -119 °F
ASTM D746