Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® L63568U Rotational Molding LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® L63568U Rotational Molding LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The resin exhibits excellent ESCR and low temperature impact strength. Formolene® L63568U is also fully UV stabilized. Formolene® L63568U meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.Applications: Toys, Medium Tanks, Playground Equipment, Drums and Agricultural and Chemical Storage TanksInformation provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Condition A, F<sub>50</sub>; ASTM D1693
ESCR 10% Igepal® 200 hour
200 hour
Condition A, F<sub>50</sub>; ASTM D1693
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.6 MPa
2700 psi
2" (50mm) per min; ASTM D638
Elongation at Yield >= 11.8 %
>= 11.8 %
2" (50mm) per min; ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
1.3mm per min; ASTM D790
Impact Test 61.0 J

@Thickness 3.17 mm,
Temperature -40.0 °C
45.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
Low Temperature; ARM
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C
122 °F
ASTM D648