Material Notes:
Description: LP 60 M is a special low porosity, high strength material based on raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a maximum density is obtained. By firing at high temperatures and using mullite as a binder, a homogeneous brick is obtained with very good refractory properties. The combination of low porosity and high mullite content results in very good abrasion resistance and corrosion resistance. Application: rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.50 g/cc
0.0903 lb/in³
Apparent
Porosity 10 %
10 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 100 MPa
14500 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.90 W/m-K

@Temperature 100 °C
13.2 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.90 W/m-K

@Temperature 650 °C
13.2 BTU-in/hr-ft²-°F

@Temperature 1200 °F
1.95 W/m-K

@Temperature 1100 °C
13.5 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
1650 °C
3000 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 60 %
60 %
Fe2O3 1.1 %
1.1 %
Na2O or K2O <= 0.50 %
<= 0.50 %
SiO2 36 %
36 %
Descriptive Properties Value Comments
Segercone 37
Thermal Shock Resistance 30 cycles
DIN 51068