Material Notes:
Silver Ink C2000808D2 is a high resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has dark color when printed and fired on float side of glass and is fully blendable with low resistance ink C2000808D1. It can be printed onto IR or UV black enamels.Silver Ink C2000808D2 is a grey ink with a pine smell at a ready to use viscosity suitable for firing on glass to form conductive tracks. The ink should be gently stirred before use avoiding the introduction of air bubbles.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 60 %
60 %
Particle Size <= 4.0 µm
<= 4.0 µm
Main Break; Fineness of Grind
<= 15 µm
<= 15 µm
3rd Streak; Fineness of Grind
Viscosity 9000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
9000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature <= 25.0 °C
<= 77.0 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.016 ohm
0.016 ohm
fired; 8 microns thick
Processing Properties Metric English Comments
Processing Temperature 150 °C
302 °F
Cure Time 7.98 - 15 min
0.133 - 0.25 hour
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 350
230 mesh stainless steel screen
Printing Mesh counts/inch 180 to 340
stainless steel or polyester screens