Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Haynes Hastelloy® W alloy, gas metal arc welds, aged 1000 hours at 650°C (1200°F)

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Haynes International, Inc.
Trade Name Hastelloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haynes Hastelloy® W alloy, gas metal arc welds, aged 1000 hours at 650°C (1200°F).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemical process industries.Data provided by the manufacturer, Haynes International, Inc.
Physical Properties Metric English Comments
Density 9.00 g/cc
0.325 lb/in³
at RT
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1055 MPa
153000 psi
565 MPa

@Temperature 760 °C
81900 psi

@Temperature 1400 °F
Tensile Strength, Yield 755 MPa
110000 psi
400 MPa

@Temperature 760 °C
58000 psi

@Temperature 1400 °F
Elongation at Break 15 %
15 %
30 %

@Temperature 760 °C
30 %

@Temperature 1400 °F
Reduction of Area 16 %
16 %
47 %

@Temperature 760 °C
47 %

@Temperature 1400 °F
Thermal Properties Metric English Comments
CTE, linear 13.2 µm/m-°C

@Temperature 20.0 - 600 °C
7.33 µin/in-°F

@Temperature 68.0 - 1110 °F
13.2 µm/m-°C

@Temperature 20.0 - 500 °C
7.33 µin/in-°F

@Temperature 68.0 - 932 °F
13.5 µm/m-°C

@Temperature 20.0 - 700 °C
7.50 µin/in-°F

@Temperature 68.0 - 1290 °F
14.2 µm/m-°C

@Temperature 20.0 - 800 °C
7.89 µin/in-°F

@Temperature 68.0 - 1470 °F
14.8 µm/m-°C

@Temperature 20.0 - 900 °C
8.22 µin/in-°F

@Temperature 68.0 - 1650 °F
15.3 µm/m-°C

@Temperature 20.0 - 1000 °C
8.50 µin/in-°F

@Temperature 68.0 - 1830 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.12 %
<= 0.12 %
Chromium, Cr 5.0 %
5.0 %
Cobalt, Co 2.5 %
2.5 %
Iron, Fe 6.0 %
6.0 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 24 %
24 %
Nickel, Ni 63 %
63 %
Silicon, Si <= 1.0 %
<= 1.0 %
Vanadium, V <= 0.60 %
<= 0.60 %