Material Notes:
Cures at low temperature. Offers strength, toughness and high temperature resistance of heat-curing film adhesives, with greater flexibility and ease of use. Can be applied to large parts with controlled meter mix operation.Applications: Structural Repair Composite Bonding Liquid Shim
Physical Properties Metric English Comments
Storage Temperature 4.00 °C
39.2 °F
Mechanical Properties Metric English Comments
Compressive Strength 78.0 MPa
11300 psi
Compressive Modulus 2.95 GPa
428 ksi
Adhesive Bond Strength >= 24.1 MPa

@Temperature 93.0 °C
>= 3500 psi

@Temperature 199 °F
Tensile Lap Shear
32.0 MPa

@Temperature -55.0 °C
4640 psi

@Temperature -67.0 °F
Tensile Lap Shear
37.0 MPa

@Temperature 25.0 °C
5370 psi

@Temperature 77.0 °F
Tensile Lap Shear
Peel Strength 9.00 kN/m
51.4 pli
Bell Peel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 70.0 °C
4.00 hour

@Temperature 158 °F
Pot Life 180 min
180 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 2 parts
Mix Ratio, Part A:Part B 100:55
Peel Strength High