Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Erhard Hippe KG
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe UP GM 205 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in mechanical and electrical applications. Very high mechanical properties at ambient temperatures. Good mechanical properties at elevated temperatures. Flame retardant.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.50 - 1.90 g/cc
1.50 - 1.90 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 120 MPa
>= 17400 psi
IEC 1212-2 5.7
Flexural Strength >= 250 MPa
>= 36300 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 10.0 GPa
>= 1450 ksi
IEC 1212-2 5.2
Compressive Strength >= 250 MPa
>= 36300 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 20.0 MPa
>= 2900 psi
Parallel to laminations; IEC 1212-2 5.6
Izod Impact, Unnotched (ISO) >= 44.0 kJ/m²
>= 20.9 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 5.00 J/cm²
>= 23.8 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
IEC 1212-2 7.2
Electrical Properties Metric English Comments
Insulation Resistance >= 5.00e+8 ohm
>= 5.00e+8 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Constant <= 4.5

@Frequency 48.0 - 62.0 Hz
<= 4.5

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 4.5

@Frequency 1.00e+6 Hz
<= 4.5

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 35000 V

@Temperature 90.0 °C
>= 35000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.050

@Frequency 48.0 - 62.0 Hz
<= 0.050

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
<= 0.050

@Frequency 1.00e+6 Hz
<= 0.050

@Frequency 1.00e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 600 V
>= 600 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Proof Tracking Index 500
IEC 1212-2 6.4
Thermal Endurance 140 T.I.
IEC 1212-2 7.1
Water Absorption < 101 mg
IEC 1212-2 8.2; Test piece 50 x 50 x 10 mm