Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Honeywell Aegis™ HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Aegis™ HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Aegis HCA73ZP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combination of strength and toughness associated with nylon 6/6,6 as well as excellent heat, chemical, and abrasion resistance. The reduced melt point (385 degF/196 degC) of this resin results in lower process melt temperature, lower head pressure, and lower amperage. This translates to higher extrusion rates and thinner nylon layer capabilities. It will also thermoform at lower temperatures and yield higher production rates.Applications:Processed MeatFresh Red MeatPoultryFishCheeseDried FoodChilled Fruit JuicesInformation provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D1505
Water Absorption 0.80 %
0.80 %
Extractable Content
1.4 %
1.4 %
in 24 hours
Moisture Absorption at Equilibrium 2.5 %
2.5 %
at 50% RH
Water Absorption at Saturation 9.0 %
9.0 %
Oxygen Transmission Rate 37.2 cc/m²/day
2.40 cc/100 in²/day
Nitrogen Transmission 7.80 cc-mm/m²-24hr-atm
19.8 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Carbon Dioxide Transmission 113 cc-mm/m²-24hr-atm
287 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Viscosity Measurement 3.0
3.0
96% SAV
73
73
FAV; ASTM D789
Maximum Moisture Content 0.080
0.080
Melt Flow 4.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
4.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
ASTM D3418
Processing Properties Metric English Comments
Middle Barrel Temperature 225 - 245 °C
437 - 473 °F
Tubular (Blown) Film
225 - 250 °C
437 - 482 °F
Cast Film
Adapter Temperature 243 °C
469 °F
Tubular (Blown) Film
250 °C
482 °F
Cast Film
Die Temperature 240 °C
464 °F
Cast Film
240 °C
464 °F
Tubular (Blown) Film
Melt Temperature 243 °C
469 °F
Tubular (Blown) Film
248 °C
478 °F
Cast Film
Moisture Content 0.080 %
0.080 %