Huntsman AroCy XU 71787.07 L Cyanate Ester

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name AroCy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman AroCy XU 71787.07 L Cyanate Ester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Comments/Applications: Toughened Dicyclopentadiene based cyanate ester resin.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 6000 - 16000 cP
6000 - 16000 cP