Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ICO Polymers ICORENEâ„¢ 150-1497 HDPE Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Rotational Molding Grade
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICORENE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICORENEâ„¢ 150-1497 HDPE Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ICORENE 150-1497 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. Applications: This ICORENE® grade is particularly suitable for use in kayak applications. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
Melt Index of Compound 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 25.30 MPa
3669 psi
2"/min; ASTM D638
Elongation at Break 611 %
611 %
2"/min; ASTM D638
Flexural Modulus 0.96499 GPa
139.96 ksi
ASTM D790
Impact 26

@Temperature -40.0 °C
26

@Temperature -40.0 °F
J/mm, instrumented impact, rotomolded test sample; ICO R&D1.14