Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Imerys ImerPlastâ„¢ 10WPC Recycled Polyolefin Resin

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyolefin
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name ImerPlast™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys ImerPlastâ„¢ 10WPC Recycled Polyolefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ImerPlast 10WPC is a black, UV stabilized, recycled resin with no significant odor, for compounding with wood flour for extruded decking applications. Melt filtered to 250 µm to ensure no particulates and offering a high coefficient of friction to extruded surfaces.Information provided by Imerys.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
1.8 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.8 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength 26.0 MPa
3770 psi
Tensile Modulus 1.20 GPa
174 ksi
Processing Properties Metric English Comments
Moisture Content 0.05 %
0.05 %
as packed
Descriptive Properties Value Comments
Color Dark Gray
Melt Filtration 250 µm
Users viewing this material also viewed the following: