Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties.. |
|||
Melt Flow | 1.8 - 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4116P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 1.8 - 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 1.8 - 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 5117P (18602) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 1.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
1.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
PTS Trilac® ABS-HH2500 Super High Heat ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 1.8 - 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4115P (16402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 1.8 - 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4117P (18402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 1.8 - 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 - 2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4118P (18402) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa HC-110 Modified ABS Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 230 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Imerys ImerPlast™ 10WPC Recycled Polyolefin Resin ImerPlast 10WPC is a black, UV stabilized, recycled resin with no significant odor, for compounding with wood flour for extruded decking applications. Melt filtered to 250 µm to ensure no particu.. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 1 HF 7740F High Density Polyethylene EX1 is a high density polyethylene with 1-Butene as co monomer. It has acceptable tear strength, medium molar mass and narrow molar mass distribution.Applications: stretched film and tapes for prod.. |
|||
Melt Flow | 1.8 g/10 min @Load 21.6 kg, Temperature 190 °C |
1.8 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene GA2850 High Density Polyethylene CHARACTERISTICS: HIGH MOLECULAR WEIGH FOR BLOW MOLDING GRADE, RIGID, STACKABLE AND HIGHLY SHOCK RESISTANT CONTAINERS, EXCELLENT IMPACT STRENGTH APPLICATIONS: BLOW MOLDING FOR L-RING DRUMS (200 LITRE.. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133/ASTM D1238 |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 38 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® TB 38 HDPE Made for tape applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and.. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® BB2581 HDPE for Blow Molding Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for h.. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 8007F-400 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, .. |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100P BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved ProcessingDelrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100P provides maximum toughness in the product line.. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-717C ABS Medium impact |
|||
Melt Flow | 1.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 1501E Description: Extrusion GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ABS 3500 EF-Low Gel Extrusion Grade, Low Gel Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 9500B Description: Blow Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ASA S124 ASA Weatherable Polymers Injection Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S210 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S210B Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Melt Flow | 1.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-757 ABS High gloss, medium impact |
|||
Melt Flow | 1.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |