Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Imerys Kaolexâ„¢ SC Kaolin

Category Ceramic , Clay , Kaolin Clay
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name Kaolex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys Kaolexâ„¢ SC Kaolin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Oil Absorption 200 - 300 %
200 - 300 %
g/100g clay; rub out method
Particle Size 1.1 µm
1.1 µm
average
Particle Mesh Size 325 Mesh
325 Mesh
1.01% retained
pH 4.0 - 5.5
4.0 - 5.5
0.28
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
Brookfield Viscosity >= 100 cP

@Temperature 25.0 °C
>= 100 cP

@Temperature 77.0 °F
20 RPM, 70% clay/water slip
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.100 ohm-cm
<= 0.100 ohm-cm
specific resistance
Processing Properties Metric English Comments
Moisture Content <= 2.0 %

@Temperature 105 °C
<= 2.0 %

@Temperature 221 °F
as produced
Descriptive Properties Value Comments
Color white
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved