Momentive Performance Materials PolarTherm® PTX25 Boron Nitride (BN) Powder

Category Ceramic , Nitride , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name PolarTherm®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials PolarTherm® PTX25 Boron Nitride (BN) Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Spherical BN Agglomeration Powder. Spherical nature may improve thermal conductivity at moderate loading levels when used as a filler in polymers or lubricants, and produce less anisotropic properties. Features of BN include thermal conductor, electrical insulator, low dielectric constant, high temperature stability, lubricious, inert, and non-wetting.Information provided by Momentive Performance Materials.
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
Tap Density
Particle Size >= 10 µm
>= 10 µm
D10
25 µm
25 µm
Mean
<= 45 µm
<= 45 µm
D90
Specific Surface Area 7.0 m²/g
7.0 m²/g
Descriptive Properties Value Comments
Carbon 0.03%
Morphology Spherical Agglomerate
Oxygen 0.2%
Sol. Borate 0.1%