Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Comparative Tracking Index | 300 V | 300 V | Test liquid A; IEC 60112 |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Comparative Tracking Index | 300 V @Thickness 3.17 mm |
300 V @Thickness 0.125 in |
ASTM D3638 |
Industrial Laminates/Norplex NP424 Laminate Description: Composite material composed of woven glass fabric surfaces and paper core combined with epoxy resin. Primarily used in the printed circuit board industry. Easy punching and excellent el.. |
|||
Comparative Tracking Index | 300 V | 300 V | d.a.m.; Solution A; IEC 60112 |
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS. |
|||
Comparative Tracking Index | 300 V | 300 V | A solution |
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
Teijin Panlite® LS-2250 Friction and Abrasion Resistant Polycarbonate Resin It is compounded with fluorine powder to improve friction and abrasion resistance, meeting UL 94 V-2. The friction and abrasion resistance is superior than that of polyamidoacetal, maintaining excel.. |
|||
Comparative Tracking Index | 300 V | 300 V | UL 746 |
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Comparative Tracking Index | 300 V | 300 V | TS EN 60112 |
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC Method |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Covestro Bayblend® FR 86 Polycarbonate/ABS Blend Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
DSM Stanyl® TW200F8 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
DSM Stanyl® TW241F10 (DAM) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Covestro Bayblend® KL 1-1430 Polycarbonate/ABS Blend Standard grade for cars.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Comparative Tracking Index | 300 V | 300 V | |
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided .. |
|||
Comparative Tracking Index | 300 V | 300 V | Test solution A; IEC 60112 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Comparative Tracking Index | 300 V | 300 V | CEI 60112/Solution A |
Addiplast Addinyl A2H M30 Flame Retardant Nylon 66, 30% Mineral Filled Flame retardant, 30% mineral filled, with halogensInformation provided by Addiplast. |
|||
Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
DSM Akulon® K223-HMS6 Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 300 V | 300 V | Test solution A; IEC 60112 |
BASF Ultradur B 4300 G2 High Speed Unc. 10% Glass Filled PBT Ultradur B 4300 G2 High Speed Unc. is a high flow, fast cycling with low warpage, 10% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable ap.. |
|||
Comparative Tracking Index | 300 V @Temperature 23.0 °C |
300 V @Temperature 73.4 °F |
IEC 60112 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Polimeri Europa KOBLEND PCA 638 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with very good impact behaviour even at low temperatures, good dimensional stability. Vicat/B50 = 120°C Main application fields: au.. |
|||
Comparative Tracking Index | 300 V | 300 V | |
Polimeri Europa KOBLEND PCA 638F PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Similar to KOBLEND PCA 638 with an improved fluidity, suitable to mould complex items. Unfilled. Suitable for Injection Molding. Supplied as pellets.ISO dat.. |
|||
Comparative Tracking Index | 300 V | 300 V | Test solution A; IEC 112 |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Comparative Tracking Index | 300 V | 300 V | Test Solution A; IEC 60112 |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Comparative Tracking Index | 300 V | 300 V | Test Solution A; IEC 60112 |
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |