Ineos ABS Lustran® 1460, Injection Grade  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® 1460, Injection Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection molding grade, increased heat and impact resistance, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Typical value for ABS
Melt Flow 5.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
Elongation at Yield 2.4 %
2.4 %
Tensile Modulus 2.40 GPa
348 ksi
Charpy Impact Unnotched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 2.40 J/cm²
11.4 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 101 °C
214 °F