Ineos ABS Lustran® QE 1110, Extrusion Grade  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® QE 1110, Extrusion Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion grade, for coextrusion to surfaces with extreme low gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Melt Flow 3.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
Elongation at Yield 2.0 %
2.0 %
Tensile Modulus 1.80 GPa
261 ksi
Charpy Impact Unnotched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 2.10 J/cm²
9.99 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Vicat Softening Point 97.0 °C
207 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm