Polymer Property : Melt Flow = 0.27 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 40 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 40 is characterized by a high melt strength leading to a good bubble stability..
Melt Flow 0.27 g/10 min
0.27 g/10 min
ISO 1133
Total Lacqtene® FB 3010 LDPE blown film  (discontinued **)
Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 180 to 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Chevron Phillips HiD® 9406 HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good Stress Crack ResistanceAppli..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Chevron Phillips HiD® 9502/HiD® 9503 with Antistat HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Excellent ESCR, High Melt Strength, Good Impact Resistance..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Chevron Phillips HiD® 9506 HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good ESCR, High Melt Strength, Good Impact Resistance, Goo..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips HiD® 9330 HDPE Natural Pipe Resin  (discontinued **)
Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: base resin for use in utility and conduit pipe applicationsI..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips HiD® 9502H - 9503H High Performance Series HDPE Blow Molding Resin  (discontinued **)
Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips Marlex® 9506H High Performance Series HDPE Blow Molding Resin  (discontinued **)
Resin Type: linear copolymerCharacteristics: superior physical properties, medium molecular weight distribution, wide range of processing conditions, low parison sag, excellent stress crack resistan..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer.
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 14A Butene MDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness, broad MW distribution.Applications: Co-extrusion, blending.Data provided by the manufacturer.
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ineos G36-24-149 MDPE with Carbon Black  (discontinued **)
Fortiflex® G36-24-149 is a black medium density polyethylene resin designed for sheet extrusion. This resin has excellent environmental stress crack resistance (ESCR) and ultra violet protection. ..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ineos G36-24-150 HDPE
Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical p..
Melt Flow 0.27 g/10 min

@Load 2.16 kg
0.27 g/10 min

@Load 4.76 lb
ISO 1133
Total Xsene® BM 593 HDPE, blow molding
FINATHENE® BM 593 is a new generation of bimodal high density polyethylene based on hexene (C6) as co-monomer and is produced by the ATOFINA Double Loop Technology™. FINATHENE® BM 593 has been es..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips Marlex® 9503HF High Performance Series HDPE Blow Molding Resin
Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene
TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Chevron Phillips HiD® 9330T HDPE Natural Pipe Resin  (discontinued **)
Resin Type: Gas Phase Linear Hexene CopolymerASTM D 4976 Classification: PE 235, A 54607ASTM D3350 Classification: 335540AApplications: Base resin for use in utility and conduit pipe applications.Da..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem TS9003 LDPE Blown Film Extrusion Polyethylene
TS9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance along with good optical properties and high stiffness. These characteristics ensure the production of packag..
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene
TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its ..