Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H03G-03 Polypropylene Homopolymer  (discontinued **)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade , Polypropylene, Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H03G-03 Polypropylene Homopolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Suggested fabrication methods: ExtrusionFeatures: Ease of processingTypical applications: Oriented filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005.
Physical Properties Metric English Comments
Density 0.886 - 0.926 g/cc
0.0320 - 0.0335 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79 - 108
79 - 108
Normal range for injection molding resins; ASTM D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.28 GPa
186 ksi
ASTM D790A
Izod Impact, Notched 0.200 - 0.300 J/cm

@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Descriptive Properties Value Comments
Process Oriented Film/Blow Molding/Fiber