Material Notes:
High melt flow, Crystal clearApplications: Razor components, Personal care, Thin wall moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optical properties of the material.Properties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 19.7 g/10 min
19.7 g/10 min
Condition G
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
Tensile Strength, Ultimate 39.0 MPa
5660 psi
ASTM D638
Elongation at Break 1.3 %
1.3 %
ASTM D638
Modulus of Elasticity 3.50 GPa
508 ksi
ASTM D638
Flexural Yield Strength 70.0 MPa
10200 psi
ASTM D790
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
ASTM D648
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.59

@Wavelength 589.3 nm
1.59

@Wavelength 589.3 nm
sodium D line
Optical Density 0.046
0.046
400-700 mm avg.
Transmission, Visible 88 - 90 %
88 - 90 %
at 550 mm
Electrical Properties Metric English Comments
Dielectric Constant 2.59

@Frequency 1e+6 Hz
2.59

@Frequency 1e+6 Hz
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
Processing Properties Metric English Comments
Melt Temperature 190 - 274 °C
374 - 525 °F
Mold Temperature 38.0 - 82.0 °C
100 - 180 °F