Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BL3VD is a high density polyethylene with 1-Butene as co monomer. It is very high density and stiffness, good ESCR, high flowability and impact strength.Applications: small blow molding, bottles, containers (up to 10 L ).Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
ISO 1183
Environmental Stress Crack Resistance 3.0 hour

@Pressure 3.50 MPa
3.0 hour

@Pressure 508 psi
ISO CD 16770
Melt Flow 1.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
2.7 g/10 min

@Load 21.6 kg,
Temperature 190 °C
2.7 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ISO 868
Tensile Stress 32.0 MPa
4640 psi
at Break; ISO 527
Tensile Strength, Yield 28.0 MPa
4060 psi
ISO 527
Elongation at Break >= 600 %
>= 600 %
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Softening Point 80.0 °C
176 °F
ISO 306
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Descriptive Properties Value Comments
Swell Ratio, % >115