Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) T 30 S Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade , Polypropylene, Fiber Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) T 30 S Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
T30S is a polypropylene homopolymer particularly suitable for the extrusion of sheet for thermoforming, film yarn and mono filament.Applications: T30S is designed for bags industrial fabrics and mates and is used for baler twines and ropes.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 3.2 g/10 min
3.2 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ISO 868
Tensile Stress 34.0 MPa
4930 psi
ISO R527
Elongation at Yield 13 %
13 %
ISO R527
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 155 °C
311 °F
ISO 306/A
Heat Distortion Temperature 110 °C
230 °F
ISO 75/B