Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 75 OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 75 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 75 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex CL 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 106 are characterized by h.. |
|||
Melt Flow | 3.2 g/10 min | 3.2 g/10 min | ISO 1133:1997 |
Nanocyl PLASTICYL™ PP2001 Polypropylene with 3.2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D-1238 |
Chevron Phillips EC6755 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Containers and lidsPackaging for foods such as yot, sour cream, delicatessen salads and gravyCold temperature packagingPortion dairy containersFe.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 210 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 410 °F |
|
Noltex Soarnol® BS3803 Ethylene Vinyl Alcohol Copolymer Modified ET3803; New Stretchable EVOH. Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows .. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 210 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 410 °F |
|
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%... |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
GRECO ISOPAK 540 ABS Resin Flame Retardant GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Melt Flow | 3.2 g/10 min | 3.2 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) T 30 S Polypropylene T30S is a polypropylene homopolymer particularly suitable for the extrusion of sheet for thermoforming, film yarn and mono filament.Applications: T30S is designed for bags industrial fabrics and mat.. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 250 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCD825 PPE-TPE (Asia Pacific) Flexible, very low-migration, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-1 re.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Silon Tabond 2005 Adhesive Resin TABOND 2005 is a plastomer modified with maleic anhydride functional groups.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon, EVOH, PET, PBT, PC, aluminium, copper, brass .. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Unipetrol PP MONSTEN® TB 003 Polypropylene Homopolymer Applications include injection molding, tapes, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 3101 Acid-/Acrylate-Modified EVA Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 175 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 347 °F |
ASTM D1230 |
Lubrizol Estane® ALR CL60D Thermoplastic Polyurethane Type: Estane® ALR CL600 is a Shore D thermoplastic polyurethane (TPU) resin.Features: Contains a UV package that enhances outdoor weatherability, but does not contain lubricants or wax processing a.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Melt Flow | 3.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics EB6755 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
3.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 75 OG General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 3.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |