Material Notes:
Information provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
Environmental Stress Crack Resistance 400 hour
400 hour
Melt Flow 5.5 g/10 min
5.5 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.0 MPa
3190 psi
Elongation at Break 400 %
400 %