Kazanorgsintez 10803-020 High Pressure Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Kazanorgsintez
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez 10803-020 High Pressure Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contact, toys, films and film articles, shaped-molded parts, etc.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.917 - 0.920 g/cc
0.0331 - 0.0332 lb/in³
Environmental Stress Crack Resistance >= 2.0 hour
>= 2.0 hour
Melt Flow 2.0 g/10 min
2.0 g/10 min
±10% Superior Quality, ±15% Premium Quality, 2nd Quality
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 9.30 MPa
>= 1350 psi
Elongation at Break >= 550 %
>= 550 %
Tear Strength Test >= 12.2
>= 12.2
MPa
Descriptive Properties Value Comments
Amount of impurities [pcs] 15
2nd Quality
2
Superior Quality
5
Premium Quality
Extractable Substance Weight Content (%) 0.9
Extra Class
1.1
1st and 2nd Class