Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kotec Carbotex KGN-30MRA Polycarbonate, Flame Retardant, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Glass Fiber Filled, Flame Retardant
Manufacturer Kotec Corp
Trade Name Carbotex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kotec Carbotex KGN-30MRA Polycarbonate, Flame Retardant, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation provided by Kotec Corporation
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Water Absorption 0.20 %

@Temperature 23.0 °C,
Time 86400 sec
0.20 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D995
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D995
Mechanical Properties Metric English Comments
Tensile Strength at Break 127 MPa
18400 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 162 MPa
23500 psi
ASTM D790
Flexural Modulus 7.55 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
V-Notched 1/8"; ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 146 °C
295 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.70 mm
V-0

@Thickness 0.0669 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.2

@Frequency 1.00e+6 Hz
3.2

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.00080

@Frequency 1.00e+6 Hz
0.00080

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 110 sec
110 sec
ASTM D495
Descriptive Properties Value Comments
Light Transmittance Translucent
3.0mm, ASTM D1003
Users viewing this material also viewed the following: