Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latistat 83-05 POM, Impact Modified

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Impact Modified
Manufacturer LATI
Trade Name Latistat
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latistat 83-05 POM, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dissipative product based on Polyamide 12 (PA12), impact modified. Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
Elongation at Break 85 %
85 %
Elongation at Yield 8.0 %
8.0 %
Tensile Modulus 1.70 GPa
247 ksi
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
Vicat Softening Point 125 °C

@Load 5.00 kg
257 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 260 ohm
260 ohm
Processing Properties Metric English Comments
Melt Temperature 180 - 210 °C
356 - 410 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 70.0 - 90.0 °C

@Time 10800 sec
158 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: