Material Notes:
Description: LUTENE-H PE0235 is a materials with high toughness and rigidity suitable for cable protection It has very high resistance to stress cracking and long-term internal pressure creep property.Applications: Cable protection pipeCAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ASTM D1505
Environmental Stress Crack Resistance >= 200 hour
>= 200 hour
F50; ASTM D1693
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Yield 23.5 MPa
3410 psi
ASTM D638
Elongation at Break >= 900 %
>= 900 %
ASTM D638
Flexural Modulus 1.08 GPa
156 ksi
ASTM D790
Izod Impact, Notched 1.96 J/cm

@Temperature 23.0 °C
3.67 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Users viewing this material also viewed the following: