Material Notes:
TLS A6 tool steel is a medium-alloy, air-hardening tool steel that is characterized by its ability to be through hardened while using the low austenitizing temperatures which are typically associated with oil-hardening tool steels. TLS A6 exhibits good toughness and excellent dimensional stability in heat treatment. TLS A6 is intermediate in wear resistance between O1 oil-hardening tool steel and D2 high-carbon, high-chromium tool steel. Typical applications for TLS A6 tool steel include blanking and forming dies, trim dies, bending and forming tools, mandrels, chuck jaws, tooling for plastic injection molding, dowel pins, shear knives, and gages.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.83 g/cc
7.83 g/cc
Density 7.83 g/cc
0.283 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 47
47
Air Cooled from 843°C, 593°C Temper Temperature
52
52
Air Cooled from 843°C, 427°C Temper Temperature
62
62
Air Cooled from 843°C, As Quenched
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 80 %
80 %
1% Carbon Steel
Izod Impact Unnotched 40.7 J
30.0 ft-lb
Air Cooled from 843°C; 150°C Temper Temperature
102 J
75.0 ft-lb
Air Cooled from 843°C; 316°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 13.1 µm/m-°C

@Temperature 21.0 - 316 °C
7.28 µin/in-°F

@Temperature 69.8 - 601 °F
14.7 µm/m-°C

@Temperature 21.0 - 704 °C
8.17 µin/in-°F

@Temperature 69.8 - 1300 °F
Component Elements Properties Metric English Comments
Carbon, C 0.70 %
0.70 %
Chromium, Cr 1.0 %
1.0 %
Iron, Fe 94.75 %
94.75 %
Manganese, Mn 2.0 %
2.0 %
Molybdenum, Mo 1.25 %
1.25 %
Silicon, Si 0.30 %
0.30 %
Chemical Properties Metric English Comments
Critical Temperature 727 °C
1340 °F
Ac1